In the picture to the right I was looking at how bad the inside surface of the skin got scratched from the top rib of the VS. It wasn't too bad so I just scotchbrited and shot it with some zinc chromate. I have decided that I am going to prime all of the internal ribs/spars/stiffeners as well as where they mate to the skin. I am using Moeller's zinc chromate at the moment. I tried both the yellow and green primers but have found the green to cover much more evenly.
The vertical stabilizer all clecoed together. Tiffany's favorite task is clecoing, good thing because it is one of my least favorites.